UTP A 6170 Co

Hersteller
Ceweld product
Type
Nickel based alloy with high heat resistance combined with excelent mechanical strength
classification
AWS
A 5.14: ERNiCrCoMo-1
EN ISO
18274: S Ni 6617(NiCr22Co12Mo9)
W.Nr.
2.4627
Anwendungen
CEWELD NiCrCo 617 is a high temperature alloy which is used for welding of nickel-chromium-cobalt-molybdenum alloys (UNS Number N06617). This filler metal can also be used for overlay cladding where similar alloy is required such as gas turbines and ethylene equipment.
Type
Nickel based alloy with high heat resistance combined with excelent mechanical strength
Anwendungen
CEWELD NiCrCo 617 is a high temperature alloy which is used for welding of nickel-chromium-cobalt-molybdenum alloys (UNS Number N06617). This filler metal can also be used for overlay cladding where similar alloy is required such as gas turbines and ethylene equipment.
Eigenschaften

Weld metal provides optimum strength and oxidation resistance above 816°C (1500°) up to 1149°F (2100°F), especially when welding on base metals of nickel-iron-chromium alloys.

Classification
AWS
A 5.14: ERNiCrCoMo-1
EN ISO
18274: S Ni 6617(NiCr22Co12Mo9)
F-nr
43
FM
6
W.Nr.
2.4627
Geeignet für

E Ni 6617(NiCr22Co12Mo), ENiCrCoMo-1, 2.4628

2.4663, 2.4851, 1.4876, 1.4859, 1.4952, 1.4958, 1.4959,

NiCr21Co12Mo, NiCr23Co12Mo, NiCr23Fe, X6CrNiNbN 25 20, X5NiCrAlTi 31 20, X8NiCrAlTi 32 21, X10 NiCrAlTi 32 21, GX10 NiCrSiNb 32 20, 

UNS: N06601, N06617, N08810, N08811

Inconel Alloys 600 and 601, Incoloy Alloys 800 HT and 802 and cast Alloys such as HK-40, HP and HP-45 Modified,  Alloy 617,

Schweißpositionen
PA
PB
PC
PD
PE
PF
PG
Rücktrocknung
Not required
Gas acc. EN ISO 14175
I1
Analyse
C Si Mn Cr Ni Mo Nb Ti V Fe W Co Cu Al P S Nb+Ta
0.1 0.8 0.8 22 55 9 0.2 2.5 13 1
Mechanische Gütewerte
Heat
Treatment
RP0,2
(MPa)
Rm
(MPa)
A5
(%)
Impact Energy (J) ISO-V Hardness
RT
As Welded 480 760 32 120 HRc
Type
Nickel based alloy with high heat resistance combined with excelent mechanical strength
classification
AWS
A 5.14: ERNiCrCoMo-1
EN ISO
18274: S Ni 6617(NiCr22Co12Mo9)
W.Nr.
2.4627
Anwendungen
CEWELD NiCrCo 617 is a high temperature alloy which is used for welding of nickel-chromium-cobalt-molybdenum alloys (UNS Number N06617). This filler metal can also be used for overlay cladding where similar alloy is required such as gasturbines and ethylene equimpent.
Type
Nickel based alloy with high heat resistance combined with excelent mechanical strength
Anwendungen
CEWELD NiCrCo 617 is a high temperature alloy which is used for welding of nickel-chromium-cobalt-molybdenum alloys (UNS Number N06617). This filler metal can also be used for overlay cladding where similar alloy is required such as gasturbines and ethylene equimpent.
Eigenschaften

Weld metal provides optimum strength and oxidation resistance above 815 °C (1500°F) up to 1149 °C (2100°F), especially when welding on base metals of nickel-iron-chromium alloys.

Classification
AWS
A 5.14: ERNiCrCoMo-1
EN ISO
18274: S Ni 6617(NiCr22Co12Mo9)
F-nr
43
FM
6
W.Nr.
2.4627
Geeignet für

E Ni 6617(NiCr22Co12Mo), ENiCrCoMo-1, 2.4628

2.4663, 2.4851, 1.4876, 1.4859, 1.4952, 1.4958, 1.4959,

NiCr21Co12Mo, NiCr23Co12Mo, NiCr23Fe, X6CrNiNbN 25 20, X5NiCrAlTi 31 20, X8NiCrAlTi 32 21, X10 NiCrAlTi 32 21, GX10 NiCrSiNb 32 20, 

UNS: N06601, N06617, N08810, N08811

Inconel Alloys 600 and 601, Incoloy Alloys 800 HT and 802 and cast Alloys such as HK-40, HP and HP-45 Modified,  Alloy 617,

Schweißpositionen
PA
PB
PC
PD
PE
PF
Rücktrocknung
Not required
Gas acc. EN ISO 14175
I1
Analyse
C Si Mn Cr Ni Mo Nb Ti V Fe W Co Cu Al P S Nb+Ta
0.1 0.8 0.8 22 50 9 0.4 2.5 13 1
Mechanische Gütewerte
Heat
Treatment
RP0,2
(MPa)
Rm
(MPa)
A5
(%)
Impact Energy (J) ISO-V Hardness
RT
As Welded 480 760 32 120 HRc