CastoDur N 9120
Outstanding alloy against abrasion, thermo-shock and corrosion combined with high temperatures. The weld deposit can be machined with tungsten tool tips and by grinding. The hardness of the weld deposit will degrees 20% at 600 °C and has a nominal hardness of 49-53 HRc at room temperature. The weld deposit is high heat resistant up to 900 °C. E Dur 12 offers a low coefficient of friction of and exceptional resistance to galling. It has cavitation-erosion resistance ten times that of 304 stainless steel, E Dur 12 can be used to protect bearing surfaces in non-lubricating conditions due to its resistance to metal-to-metal wear.
46-48 HRc, Stellite 12 Alloy with high temperature and abrasion resistance, Thermo shock resistant and impact resistant, Hardfacing valves, Seats, Pumps, Knives, Plastic recycling crushers etc.
Heat Treatment |
RP0,2 (MPa) |
Rm (MPa) |
A5 (%) |
Hardness |
---|---|---|---|---|
As Welded | 49 HRc |