Special alloy with age hardenable deposit and similar mechanical properties as the base metal. Age hardened condition: 720ºC for 8 Hours, furnace Cool 55ºC/hour to 620ºC than Air Cool for 8 hours
Inconel 718(2.4668), 706 and X-750 (X750)
Heat Treatment |
RP0,2 (MPa) |
Rm (MPa) |
A5 (%) |
Hardness |
---|---|---|---|---|
As Welded | 580 | 860 | 28 | HRc |