Properties of the #1 underwater wet welding electrode, AquaForce

We have achieved a breakthrough in developing a new electrode for wet welding, after a long and challenging process. It took us nearly 7 years and over 200 formulations to create the best electrode for underwater wet welding. We are proud to introduce CEWELD® AquaForce HR and CEWELD® AquaForce MG, the latest additions to our CEWELD® AquaForce family. These electrodes meet the standards of DIN 2302 (which will soon become an ISO standard) and AWS A 5.35 and AWS D 3.6M.

Exclusive try discount On your first order!*

* Regardless of the order quantity
* For new costumers only

Shipping adress
Remote video URL
Remote video URL
UNDERWATER WELDING

The term "underwater welding" is used to describe welding work carried out under various ambient conditions in which the workpieces to be welded are located below the surface of the water.

Earl Toups, Hyperbaric Welding and NDT Manager at DCN Diving  explains how it feels to weld underwater.

CEWELD® AquaForce

CEWELD® AquaForce Electrodes are designed for hyperbaric, wet underwater welding

Direct contact of arc and workpiece with the water.

  • it is the key technology for repairing underwater steel structures that cannot go into dry dock.
  • Welding is performed underwater and is directly exposed to the wet environment.
  • The greater flexibility makes it more effective, efficient and economical than long stays in the shipyard with laborious evacuation of the water.
  • Power is supplied by cables and hoses connected to the welder.
  • Complete insulation of the cables and hoses is essential to avoid the risk of electric shock.
  • SMAW (Shielded metal arc welding) is one of the most commonly used methods in repair welding.
Image
underwater welding electrode AquaForce
CEWELD® AquaForce The #1 electrode for wet welding!
Image
Aquaforce Underwater wet welding electrode
  • Beautiful fine rippled and smooth bead appearance
  • Self lifting slag
  • Extreme stable arc with excellent weld pool visibility
  • No metal-powder in the coating
  • No porosity, No inclusions
  • 3,2 mm offers easily an A height of 4 mm in all positions
  • No concave welds in any position
  • No grinding necessary between the layers
  • Environmentally friendly insolation that contains no Vinyl, Acryl, Alkyd or Paraffin 
CEWELD® AquaForce HR
STANDARD CLASSIFICATION EN ISO 2560-A : E 42 2 RB 4 1
DIN 2302 : E 42 2 Z RB 10 fr
AWS 5.1 : E 7014
AWS 5.35 : UWE 7014 1A

 

TYPICAL ANALYSIS OF THE PURE WELD METAL (%)

C Mn Si P S
0,075 0,75 0,6 < 0,025 <0,025

 

TYPICAL QUALITY VALUES OF THE PURE WELD METAL ACCORDING TO ISO

      Charpy V J (ft-lbf) ISO-V  
Rp0,2 MPa (ksi) Rm MPa (ksi) 20°C (-4°F) 0°C (0°F) -20°C (-4°F)
> 420 (67) 500 - 640 (78 - 95)   52 (50) -
CEWELD® AquaForce MG
STANDARD CLASSIFICATION EN ISO 2560-A : E 42 2 RR 4 1
DIN 2302 : E 42 0 Z RR 10 fr
AWS 5.1 : E 7013
AWS 5.35 : UWE 6013 2A

 

TYPICAL ANALYSIS OF THE PURE WELD METAL (%)

C Mn Si P S
0,08 0,60 0,40 < 0,025 <0,025

 

TYPICAL QUALITY VALUES OF THE PURE WELD METAL ACCORDING TO ISO

      Charpy V J (ft-lbf) ISO-V  
Rp0,2 MPa (ksi) Rm MPa (ksi) 20°C (-4°F) 0°C (0°F) -20°C (-4°F)
> 420 (67) 500 - 640 (78 - 95)   > 36 (27) -
Download the CEWELD® AquaForce brochure

Are you looking for a reliable and high-performance electrode for underwater welding? Do you want to join, repair, or reinforce steel structures in fresh or salt water up to 20 meters deep? Than you really need to try CEWELD® AquaForce yourself!

CEWELD® AquaForce is the preferred choice of professional divers and welders who demand quality and efficiency. Don’t settle for less than the best. Download the brochure now and discover how CEWELD® AquaForce can help you achieve your underwater welding goals!

Don’t wait any longer, experience the difference of this electrode for yourself!

Get in touch with our sales team today and find out more!
info@certilas.nl